Emissions And Stack Differential Scanning Analyzer

Emissions And Stack Differential Scanning Analyzer products with the highest accuracy of one, the sensor is the use of imported material E-couple, high precision, high sensitivity, good repeatability, signal acquisition circuit shielding protection, strong anti-interference, baseline stability and repeatability is very high.

Category:

Overview

Emissions And Stack Differential Scanning Analyzer products with the highest accuracy of one, the sensor is the use of imported material E-couple, high precision, high sensitivity, good repeatability, signal acquisition circuit shielding protection, strong anti-interference, baseline stability and repeatability is very high. The differential scanning calorimeter can be glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature and product stability, oxidation induction period and other tests. It is qualified for the research of pipe, polymer, chemical, food, medical and other fields, and serves universities, enterprises, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.

 

Features

  • 7 in (17.78 cm) touch screen for rich information display
  • New furnace design, high accuracy, uniform heating
  • USB communication, reliable and uninterrupted connection
  • Automatic dual airflow, fast switching, added protective gas
  • Simple and user-friendly software
  • Ultra-high sensitivity and accuracy: 0.001 MW, 32.0 ̊F (0.001 ℃)
  • Superior performance, cost-effective, widely used

 

Technical Specifications

Temperature range room temperature to 1022 ̊F (550 ℃)
Temperature resolution 32.0 ̊F (0.001 ℃)
Temperature fluctuation ± 32.0  ̊F (± 0.001 ℃)
Temperature repeatability ± 32.0  ̊F (± 0.01 ℃)
Heating rate 32.1 ̊F to 176 ̊F (0.1 ℃ to 80 ℃) or min
Constant temperature time Program setting ≤ 24 h
Temperature control mode heating, constant temperature, cooling (automatic program control)
DSC range 0 mW to ± 600 mW
DSC resolution 0.01 uW
DSC sensitivity 0.001 mW
Power supply AC 220 V or 50 Hz or customized
Atmosphere control gas nitrogen, oxygen (program setting or automatic switch)
Gas flow 0 ml to 300 ml or min
Gas pressure 0.2 mpa
Display mode 24-bit color, 7 in (17.78 cm) LCD touch screen display
Cooling device air cooling device (optional semiconductor & LT; – 40 ̊F to 1022  ̊F (- 40 ℃ to 550 ℃) & gt ; Liquid nitrogen refrigeration < – 238  ̊F to 1022  ̊F (< – 150 ℃ to 550 ℃ & gt)